John WilsonHypersolid Metal Tech Co., Ltd is a very responsible company that can effectively solve our problems. I hope there will be opportunities to work together in the future.
-
miaThis company is the best I have ever seen. The company's employees are particularly enthusiastic and able to respond and meet our needs. If there is a need in the future, I will still work with you!
High Purity Customized Molybdenum Lanthanum Tzm Mola Molybdenum Lanthanum Alloy Sheet

Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xCharacteristic | High Temperature Resistant | Heat Treatment | Annealing, Quenching, Tempering, Etc. |
---|---|---|---|
Material | Molybdenum Alloys | Surface Condition | Polished |
Temperature | 1800C | Thermal Conductivity | 138 W/mK |
Type | Alloy | Yield Strength | 590 MPa |
High Light | high purity molybdenum alloys,customized molybdenum alloys |
1,Description:
Molybdenum Lanthanum offers enhanced properties compared to pure molybdenum, making it a popular choice in specific applications. It exhibits excellent high-temperature strength, good thermal conductivity, and resistance to oxidation and corrosion. These properties make it suitable for use in furnace components, heating elements, and other applications that require materials capable of withstanding extreme temperatures and harsh environments.
The addition of lanthanum oxide to molybdenum improves its recrystallization temperature, creep resistance, and overall mechanical properties. This composite material retains its strength and stability even at elevated temperatures, making it ideal for applications in industries such as aerospace, energy, and metallurgy.
2,Specifications:
Density | 9.8 - 10.2 g/cm³ |
Melting Point | 2,617°C (molybdenum) |
Thermal Conductivity | 120 - 140 W/m·K |
Coefficient of Thermal Expansion | 5.2 - 6.0 x 10^-6 /°C |
Electrical Conductivity | 26% IACS (International Annealed Copper Standard) (molybdenum) |
Hardness (Vickers) | 220 - 240 HV |
Tensile Strength | 580 - 750 MPa |
Yield Strength | 400 - 550 MPa |