John WilsonHypersolid Metal Tech Co., Ltd is a very responsible company that can effectively solve our problems. I hope there will be opportunities to work together in the future.
-
miaThis company is the best I have ever seen. The company's employees are particularly enthusiastic and able to respond and meet our needs. If there is a need in the future, I will still work with you!
Mo1, Mo-La, TZM Molybdenum Rod Electrodes Chemical Cleaned Surface

Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xName | Molybdenum Rod Electrodes | Application | Automotive, Aerospace, And Electronic Appliance |
---|---|---|---|
Feature | High-temperature Strength | Surface | Chemical Cleaned |
Specifications | According To Customer Requirements | Material | Mo1, Mo-La, TZM |
High Light | TZM Molybdenum Rod,TZM Molybdenum Electrodes,Chemical Cleaned Molybdenum Electrodes |
Mo1, Mo-La, TZM Molybdenum Rod Electrodes Chemical Cleaned
Molybdenum Rod Electrodes Application
1) Used for glass industry, the fields of rare earth industry, refractory fiber industry and so on.
2) Used as vacuum material, cathode for emitting tube, and high temperature electrodes etc.
Product parameters:
Molybdenum electrodes are used for welding processes, e.g. in resistance welding. TZM (titanium-zirconium-molybdenum) is made from molybdenum by adding small amounts of small carbides.
Appearance: silver gray metallic luster
Density:>10.2g/cm
Purity: Mo>99.95%
Specifications:according to customer requirements or drawings, accept customized products.
Molybdenum electrode without defects (missing surface, missing angle, diaphragm layer, cracks)
Molybdenum electrode folding or adjustment according to user’s needs.
Atomic number |
42 |
CAS number |
7439-98-7 |
Atomic mass |
95.94 [g/mol] |
Melting point |
2620 °C |
Boiling point |
4639 °C |
Density at 20 °C |
10.22 [g/cm] |
Crystal structure |
Body-centered cubic |
Coefficient of linear thermal expansion at 20 °C |
5.210-6[m/(mK)] |
Thermal conductivity at 20 °C |
142 [W/(mK)] |
Specific heat at 20 °C |
0.25 [J/(gK)] |
Electrical conductivity at 20 °C |
17.9106[S/m] |
Specific electrical resistance at 20 °C |
0.056 [(mm2)/m] |