xDimension | Customized | Grades | Mo1 /Mo2 |
---|---|---|---|
Melting Point | 2623°C | Purity | 99.95% |
Standard | ASTM, AMS | Surface Treatment | Polished/Black Surface |
Thread Diameter | M5 M8 M10 M12 | Wall Thickness | 5~30 Mm |
High Light | customized molybdenum machining parts,pure molybdenum machining parts,high temperature molybdenum machining parts |
1,Description:
-
Molybdenum parts are widely used in various industries, including aerospace, electronics, energy, and high-temperature applications, due to their excellent strength, heat resistance, and corrosion resistance.
-
These parts exhibit a high melting point, making them suitable for use in environments with extreme temperatures.
-
Molybdenum parts possess excellent thermal conductivity, allowing for efficient heat transfer in applications such as heat sinks and furnace components.
-
With their high density, Molybdenum parts are often used in radiation shielding and counterweights for balancing machinery and equipment.
-
The mechanical properties of Molybdenum parts, such as high tensile strength and good ductility, make them suitable for use in structural components and load-bearing applications.
-
Molybdenum parts can be machined, formed, and fabricated into various shapes and sizes, providing versatility in design and application.
2,Specifications:
Physical Property | Value |
---|---|
Melting Point | Approximately 2,620°C |
Density | 10.2 g/cm³ |
Thermal Conductivity | 138 W/m·K (at room temperature) |
Coefficient of Thermal Expansion | 4.8 x 10^-6 /°C (in the range of 20-1000°C) |
Electrical Conductivity | 31% IACS (International Annealed Copper Standard) |
Hardness (Rockwell C) | 30 - 35 HRC |
Tensile Strength | 580 - 820 MPa |
Yield Strength | 340 - 690 MPa |
Elongation at Break | 10 - 30% |